Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-547 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-0504 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-0508 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-049 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-0216 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-02167 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-0747 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-1868 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-1804 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-0747 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-0216 |
filingDate |
2017-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43afd49b90c165db75db5368a2a3cdf1 |
publicationDate |
2018-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2018084159-A1 |
titleOfInvention |
Solar cell, method for manufacturing same, and solar cell module |
abstract |
A solar cell (105) is provided with a rectangular crystal silicon substrate (15). The crystal silicon substrate has a rectangular first main surface (81) and a rectangular second main surface (82). The first main surface and/or the second main surface is coated by a thin film. The thin film is formed so as to extend onto a first side surface (91), which is one of the side surfaces connecting a long side of the first main surface and a long side of the second main surface, and so as to not extend onto a second side surface (92), which is the other side surface. An oxide film (50) of silicon is provided across the whole of the surface of the second main surface in the thickness direction of the silicon substrate. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111755537-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020072271-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020509596-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020189562-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020189240-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11374141-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3940794-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3961730-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11257968-B2 |
priorityDate |
2016-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |