Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_78ca80ad4b743c901ec136b21263f093 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2253-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2257-504 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02C20-40 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28073 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28019 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-3057 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B21-0605 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28064 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B21-06 |
filingDate |
2017-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51db1744e75191f5affca370489cca6e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_908989665bee6b2648322cb1983e069f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c27e227ff12387cc36ef246e319b2ead http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c155a9d63829bf7bc2484bf1056d8c8 |
publicationDate |
2018-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2018037322-A1 |
titleOfInvention |
Rod-shaped mesoporous carbon nitride materials and uses thereof |
abstract |
Methods of producing rod-shaped mesoporous carbon nitride (MCN) materials are described. The method includes (a) obtaining a template reactant mixture comprising an uncalcined rod-shaped SBA-15 template, a carbon source compound, and a nitrogen source compound; (b) subjecting the template reactant mixture to conditions suitable to form a rod-shaped template carbon nitride composite; (c) heating the rod-shaped template carbon nitride composite to a temperature of at least 500 °C to form a rod-shaped mesoporous carbon nitride material/SB A-15 (MCN-SBA-15) complex; and (d) removing the SBA-15 template from the MCN-SBA-15 complex to produce a rod-shaped mesoporous carbon nitride material. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114763258-A |
priorityDate |
2016-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |