Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_80fe4977fb849d303e16d085f3c8c244 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2523-69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2523-27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G41-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G41-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-30 |
filingDate |
2016-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ab8b4ac277e43b950b06307c9b398f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_33d9f3257d3f2f75902b7dc209cf657f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2af2ed0470e038a28477cdd1f4a9770f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c086f55439cf46cce6f635dabc49d786 |
publicationDate |
2017-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2017219381-A1 |
titleOfInvention |
Znwo4 photocatalytic material containing oxygen deficiencies and method for preparing same |
abstract |
A ZnWO 4 photocatalytic material containing oxygen deficiencies. For ZnWO 4 containing oxygen deficiencies, absorption exists in a near infrared region of an ultraviolet-visible diffuse reflectance spectrum, wherein the wavelength range of the near infrared region is 780-2500 nm. The invention also relates to a method for preparing the ZnWO 4 photocatalytic material containing oxygen deficiencies, comprising: using NaWO 4 and a soluble zinc salt as raw materials; subjecting the raw materials to a hydrothermal crystallization reaction to generate ZnWO 4 crystals; and then roasting the ZnWO 4 crystals in the presence of hydrogen to partially reduce ZnWO 4 , so as to obtain a ZnWO 4 photocatalytic material containing oxygen deficiencies. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113173665-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113173665-A |
priorityDate |
2016-06-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |