Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ee0865b280e738c5177c93517d2c3c7b http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c0c22533c7d145dac1210effc398763c |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-28 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-06 |
filingDate |
2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e5046de7f76f4f07f2d9c1621586a0af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_155d7834e663e7c467fe88ce4cc00520 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b3ec8e3aa52ff870141a243c268c8c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0289fe9edd35d147c80d212b36769af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ddc621b3eac8acceb5da7e14d0ac47e1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53c4580185ccaa74b178983c92c6f59a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8555f6e03d7007c90a4909c2bbb31fc2 |
publicationDate |
2017-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2017186714-A1 |
titleOfInvention |
Method of forming wrinkle finish coating on a metal substrate |
abstract |
The present invention relates to a method of forming a wrinkle finish coating on a metal substrate at an installation site with the appearance similar to that of the wrinkle finish formed by applying a base paint A1 in a factory, in which method a coating composition A2 is obtained by adding 0.1–20 parts by mass of silica particulate with an average particle diameter of 0.1 µm–40 µm per 100 parts by mass of the solids in base paint A1 to the base paint A1, the coating composition A2 is applied to the metal substrate at the installation site of said component that is the object of wrinkle finish coating, and then heat-cured. Using this method, scratches, etc. that occur in a patterned coating like a wrinkle finish coating during transport and work can be easily repaired at an installation site. |