abstract |
The present invention provides: an assembly obtained by bonding a thermoplastic resin sheet and a sheet that comprises a modified block copolymer hydride in which an alkoxy silyl group is introduced, wherein the peel strength of the bonding surface is 4 N/cm or higher; a method for producing an assembly, the method including a step (1) for performing an activation process on the bonding surface of the thermoplastic resin sheet using at least one selected from the group consisting of plasma radiation, excimer ultraviolet radiation, and corona discharge, and a step (2) for superposing the bonding surfaces of the thermoplastic resin and the sheet that comprises a modified block copolymer hydride and performing thermocompression bonding; and a sheet comprising a modified block copolymer hydride in which an activation process is performed on at least one surface using at least one selected from the group consisting of plasma radiation, excimer ultraviolet radiation, and corona discharge. |