http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017130864-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cafd31a6755a3df60e0d8beb6dbbc8db |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D143-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1618 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D143-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2017-01-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dab0bbf0703845f3796b2a7537647298 |
publicationDate | 2017-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2017130864-A1 |
titleOfInvention | Antifouling coating composition, coating film, and coating-film-attached base material |
abstract | The present invention is an antifouling coating composition comprising (A) a silyl acrylic copolymer that has a constituent unit (a1) derived from triisopropylsilyl (meth)acrylate and a constituent unit (a2) derived from a polymerizable monomer having a polymerizable double bond, (B) a lower alcohol that has 1 to 3 carbon atoms, (C) an antifouling agent that contains a copper component and a zinc component and (D) a monocarboxylic acid compound, wherein the content of the lower alcohol (B) in the antifouling coating composition is 0.1 to 3% by mass. The present invention provides: an antifouling coating composition for forming a coating film which is dissipated in a reduced amount under a condition where the coating film is in contact with water at ambient temperature of about 25ºC as well as a condition where the coating film is in contact with water at a higher temperature of about 30ºC and which can maintain the physical properties thereof for a long period; a coating film produced by curing the antifouling coating composition; a coating-film-attached base material which comprises a base material and the above-mentioned coating film formed on the base material; and a method for producing the coating-film-attached base material. |
priorityDate | 2016-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |