Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_78ca80ad4b743c901ec136b21263f093 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e7f92cb7061ffc994f1f576913e8c81a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_678029c6cae2388c029ba18582f53eba http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ccbd10d41e0519a2d33ff38a846cb9e3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-52 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1057 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C37-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07G1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C45-59 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C41-01 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C39-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C39-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C45-59 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C47-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07G1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C39-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C37-54 |
filingDate |
2016-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fce673340e0e3507e4a8b12a05078b8a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec1f26ea4c3cb13223126879f00a7f0a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51602acab9d67d70acf61b5793c08cc1 |
publicationDate |
2017-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2017095555-A1 |
titleOfInvention |
Zeolite catalyst for lignin to phenol conversion |
abstract |
A method for converting lignin to a phenol product, the method comprising contacting a zeolite catalyst with a lignin under reaction conditions sufficient to produce the phenol product at a yield of equal to or greater than about 50%. A method for converting lignin to a mixed phenol product, the method comprising contacting a large-pore zeolite catalyst with a Kraft lignin under reaction conditions comprising a reaction temperature of from about 550 °C to about 850 °C to produce the mixed phenol product at a yield of equal to or greater than about 50%. |