Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ee1c19da359446fb5c4f0458a57b783d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2605-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-726 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-75 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10036 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-326 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-3405 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10165 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B17-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-34 |
filingDate |
2016-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_28737b4409fe60a12c8369f0d3ae1886 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4475dac817c6a2962b970f21fa65823e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1eb8304d2058a3bbffaf030efe523041 |
publicationDate |
2017-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2017047524-A1 |
titleOfInvention |
Antifogging product and vehicle glass |
abstract |
To provide an antifogging product and vehicle glass having a favorable appearance and satisfying favorable antifogging and peel resistance. An antifogging product provided with a transparent substrate and an antifogging layer provided on the transparent substrate as an epoxy resin cured product having constituent materials including silicon atoms and aluminum atoms, wherein the antifogging product is characterized in that, in the antifogging layer, the antifogging time (T 35 ) in a 35℃ steam test measured using a specific method is 80 seconds or longer, the variance ΔH in the haze value after the taper abrasion test stipulated in JIS R3212 is 4.0% or less, and the variance ΔYI in yellowing defined in JIS K7373 after being held 500 hours at 100℃ is 3 or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022260146-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023058561-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7210812-B1 |
priorityDate |
2015-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |