Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7a79a7677fc46be7e83ab1f3e065ed31 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A24B15-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A24B15-165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A24C5-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A24B3-14 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A24C5-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A24B3-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A24B15-14 |
filingDate |
2016-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d8781ffb31cebfdde519cac4ff01d7f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1feb558b96c746fb1fbe119d870d0ee6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5280acb887e3eff61615c9322b1e06ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1b0dfcd39c46fb00f5b16e8f63f7697 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3288c108b6bbe1435e361498758279c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d688da4856e7d3f75be1105e212f817 |
publicationDate |
2017-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2017041920-A1 |
titleOfInvention |
Method of producing high tensile strength homogenized tobacco material |
abstract |
A method of forming homogenized tobacco material comprises the steps of forming a homogenized slurry (104) comprising tobacco powder,casting the homogenized slurry onto a moving belt(105), applying a porous reinforcement sheet(205) to the surface of the cast homogenized slurry (201) such that the porous reinforcement sheet becomes incorporated into the cast homogenized slurry, and drying the cast homogenized slurry with the incorporated cellulose sheet (207) to form the homogenized tobacco material. The porous reinforcement sheet has anisotropic properties such that it has a higher tensile strength in its longitudinal direction than in its transverse direction.In this way the strength of the homogenized tobacco sheet may be significantly improved compared with prior art methods of manufacture without altering the overall composition of the homogenized tobacco material to any significant degree. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111182799-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7288444-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2800854-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021105431-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019086417-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019086462-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190093440-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112399801-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020002663-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11753750-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11712059-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112334020-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019151695-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112334020-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102367431-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112399801-B |
priorityDate |
2015-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |