http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016153610-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b817281c05ac900a51077be51df4ef14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G75-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-0254 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J19-00 |
filingDate | 2016-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58529f67cfa8160b4b9283f6f254b116 |
publicationDate | 2016-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2016153610-A1 |
titleOfInvention | Technique for forming a high melt viscosity polyarylene sulfide |
abstract | A method for forming a high melt viscosity polyarylene sulfide is provided. The method comprises reacting a sulfur source with a dihaloaromatic compound during a first stage to form an arylene sulfide prepolymer having halogen end groups; and thereafter, reacting the arylene sulfide prepolymer with a secondary sulfur source during a second stage to form the polyarylene sulfide. |