Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_75e5307f85f1b22ba0fefa73e2a89c36 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0082 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0585 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0585 |
filingDate |
2015-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b88fe66220ddd0e3a4cea4f461946bff |
publicationDate |
2016-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2016001584-A1 |
titleOfInvention |
Solid-state battery including an electrolyte made of a cross-linked solid polymer material |
abstract |
The invention relates to a method for manufacturing a thin-layer solid-state battery including the following consecutive steps: a) depositing a layer including at least one anode material on the conductive substrate thereof; b) depositing a layer including at least one cathode material on the conductive substrate thereof; c) depositing on at least one layer obtained in step a) and/or b) a layer including at least one solid electrolyte material having a thickness smaller than 10 µm, preferably smaller than 5 µm, and even more preferably smaller 2 µm, the solid electrolyte material including a cross-linked solid polymer material comprising ion groupings; d) consecutively stacking the following face-to-face: either a layer of anode material coated with a layer of solid electrolyte material obtained in step c) with a layer of cathode material optionally coated with a layer of solid electrolyte material obtained in step c), or a layer of cathode material coated with a layer of solid electrolyte material obtained in step c) with a layer of anode material optionally coated with a layer of solid electrolyte material obtained in step c); and e) performing a thermal treatment and/or a mechanical compression of the stack obtained in step d) in order to obtain a thin-layer solid-state battery. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020249877-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019215410-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3890077-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3110774-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107331534-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019215411-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3111741-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021260565-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021260571-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019215406-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3105592-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019215407-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3111740-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3097370-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021198843-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3091036-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020136313-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021234585-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021130697-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-3080862-A1 |
priorityDate |
2014-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |