abstract |
A polymer composition may include polyolefin having a molecular weight distribution of greater than or equal to 8 as measured by GPC and a metallic acrylate salt. The polymer composition may be characterized by one or more of: a melt flow rate of from 0. Ig/lOmin to 10 g/lOmin min; a melt flow viscosity between 2,000 Pa.s and 6,000 Pa.s; a die swell of between 2 and 8; and a die swell characteristic time of between 0.3 seconds and 1.2 seconds. The polymer composition may be in the form of foam. A process of forming foam may include supplying polymer composition including metallic acrylate salt and polyolefin resin, and mixing the polymer composition with foaming agent. A foam may include a polymer composition that includes polyolefin and polar polymer and does not include an ionomer. The foam may have a foam density of less than 0.25 g/cc. |