Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00644 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-0073 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate |
2015-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e470e97c318f78ac1a1d41a3889cfd45 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a5957670f3f2e84e28d7c6eab7f45d35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_caa069bd47b6abe8be05b553c21e8297 |
publicationDate |
2015-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2015137250-A1 |
titleOfInvention |
Method for producing polarizing plate |
abstract |
Provided is a method for producing a polarizing plate, which comprises: a first step wherein a protective film is bonded to one surface of a polarizing film with an aqueous adhesive layer being interposed therebetween and a releasing film is laminated on the other surface of the polarizing film with a layer of a volatile liquid being interposed therebetween; and a second step wherein the aqueous adhesive layer is dried and the volatile liquid is volatilized by heating. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10029449-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108369307-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017104463-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016540259-A |