http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015111193-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f1192a135e4bc40a5f201a9646f20172 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-134 |
filingDate | 2014-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b59607efd4d54359b1934ef56030731f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9aae417750747433542fbe92805b8f6d |
publicationDate | 2015-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2015111193-A1 |
titleOfInvention | Electrical device |
abstract | [Problem] To provide a means whereby an electrical device such as a lithium-ion secondary battery that has a positive electrode using a solid-solution positive-electrode active material can be provided with satisfactory performance in terms of rate characteristics while sufficiently making use of the high capacity characteristics that characterize solid-solution positive-electrode active materials. [Solution] An electrical device that has an electricity-generating element containing the following: positive electrodes each obtained by forming, on the surface of a positive-electrode collector, a positive-electrode active-material layer containing a positive-electrode active material; negative electrodes each obtained by forming, on the surface of a negative-electrode collector, 3 to 11 mg/cm 2 of a negative-electrode active-material layer containing a negative-electrode active material; and separators. The negative-electrode active-material layer contains the negative-electrode active material represented by formula (1), the positive-electrode active-material layer contains the positive-electrode active material (solid-solution positive-electrode active material) represented by formula (2), and a solid-solution positive-electrode active material having the composition represented by formula (3) is used as the solid-solution positive-electrode active material in the positive-electrode active-material layer. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7328219-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021504882-A |
priorityDate | 2014-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 131.