Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_df2d22103b4e46a2e14cf4143d8129de |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0085 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0569 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0569 |
filingDate |
2014-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68eff6323f0e34741e1d805e09f8b47c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8a3ab1574495fb51418aa30a95be590 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5681cf1a60fcd2a69a9e7c7344d59cf4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1611da6c7b0b8d4de65dba8270de300c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4f06c1de514d907d325d8687e1b6f9f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9dd0c84687749c140d9aef759a430374 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fa50c1adc3d49ac41c9f23b55730384 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_478740400e015faaa29d4988f365fb4f |
publicationDate |
2015-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2015104727-A1 |
titleOfInvention |
Polymer electrolyte membranes and process for the production thereof |
abstract |
The process for the production of a polymer electrolyte membrane, comprises the successive steps of: preparing a mixed solution of a Room Temperature Ionic Liquid (RTIL), at least one alkaline metal salt and a photosensitive hydrogen abstracting component at a temperature in the range 20 to 70 °C, wherein the RTIL is a compound consisting of at least one organic cation and at least one organic or inorganic anion; adding to the solution a polymeric material at a temperature in the range of 20-70 °C; blending the solution added with the polymeric material at a temperature in the range of 70-140 °C to get a uniform mixture; pressing the mixture between two sheets at a temperature in the range of 60 - 150 °C and a pressure in the range of 20 - 80 bar, so that a film is formed; and exposing the film to UV light, so that the polymeric material of the film is cross-linked and the polymer electrolyte membrane is obtained. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019052648-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106289554-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106289554-B |
priorityDate |
2014-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |