abstract |
A self-luminous coating/printing ink cured on a tyre by radiation, comprising the following components in parts by mass: 8-18 parts of acrylates, 0-8 parts of a resin, 0.5-3 parts of a rubber, 0.01-0.12 parts of a dispersing agent, 2-4 parts of a noctilucent powder, and 0.03-0.1 parts of a levelling agent. The preparation method comprises the steps of stirring acrylates and a rubber into a transparent liquid, cooling to room temperature; adding a resin and a dispersing agent, stirring; and then adding a noctilucent powder, a levelling agent and an optical initiator, and stirring for 10-30 minutes. |