Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-26 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-282 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-262 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D127-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D127-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F214-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F214-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-03 |
filingDate |
2014-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61426de7bd08f33fd1ae147a28202e82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e4a55cb4bdbcf36613cbd9b880ccd05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c710a2a60314569fc650efafc735bef8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b709ea2f5ed4c16bb5030bccca24ec5 |
publicationDate |
2015-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2015002824-A1 |
titleOfInvention |
Melt-processible vinyl fluoride interpolymers of low crystallinity |
abstract |
In a first aspect, a melt-processible interpolymer consists essentially of units derived from vinyl fluoride and at least two highly fluorinated monomers, at least one of the highly fluorinated monomers introducing into the polymer a side chain of at least one carbon atom. The interpolymer has a melt flow rate in a range of from about 2 to about 250 grams per 10 minutes at a temperature of 280 °C. In a second aspect, an emulsion polymerization process for preparing a melt-processible interpolymer includes polymerizing vinyl fluoride and at least two highly fluorinated monomers in water with a water-soluble free-radical initiator at a temperature in the range of from about 60 to about 100 °C and a pressure in the range of from about 1 to about 12 MPa. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015175271-A1 |
priorityDate |
2013-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |