http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014149423-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03ef317b4c382523de575d44d0a1c8bf |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2852 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J167-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-38 |
filingDate | 2014-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_605541dc3d83afbf9c5e651e1c5d7b9a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2fd9d775e1e5a3f90ab5bba19978115 |
publicationDate | 2014-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2014149423-A1 |
titleOfInvention | Polyester-based, pressure sensitive adhesive |
abstract | A pressure sensitive adhesive (PSA) comprising: (A) 50 to 99 weight percent (wt%) of a partially aromatic polyester comprising at least two hydroxyl groups per polymer chain and having a: (1) Storage modulus of > 0.33 Megapascals (MPa) at 23°C, (2) Mn of 20,000 to 200,000 grams per mole (g/mol), and (3) Glass transition (Tg) temperature of ~60°C to 20°C; (B) 1 to 40 wt% of at least one of a plasticizer or tackifier; and (C) 0.1 to 10 wt% of a crosslinker with a functionality of > 2.5; with the provisos that the PSA has a: (i) Tg of -60°C to 10°C; (ii) Storage modulus of <0.33 MPa at 23°C; (iii) Rubbery plateau in excess of its Tg; and (iv) Melt flow in excess of 70°C. |