http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014119533-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4283a2f8ade5dc582d75300427a38e50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G59-26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-26 |
filingDate | 2014-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3d17b672893c8230d63a32f3584f962 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_badb9991d82b17b4e5051d7b4b266a45 |
publicationDate | 2014-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2014119533-A1 |
titleOfInvention | Epoxy resin, method for producing epoxy resin, epoxy resin composition, and cured article |
abstract | The purpose of the present invention is to provide an epoxy resin which does not release a compound that is suspected as an endocrine disrupter, and which can be used as a material for a cured article having excellent surface hardness, chemical resistance, light resistance and flexibility.nThe epoxy resin according to the present invention is represented by general formula (1) [wherein A represents a structural unit having a heterocyclic ring], and is characterized by having a number average molecular weight of 400 to 100000. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016193032-A1 |
priorityDate | 2013-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 235.