abstract |
A method for making a cordierite filter article, including: firing an extruded green body batch composition according to: a first temperature ramping from ambient temperature up to a first soaking temperature; a first soaking at a temperature of at least 1255 °C for at least 2 hours; a second temperature ramping from the first soak temperature down to a second soak temperature; and a second soaking at a temperature of at least 1250 °C and at least 5 °C below the first soaking temperature, as defined herein. |