Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8a9982b1666c54b5bf02d6c944891e4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d8fbc46a856fc7651583fa73d6856e2e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2218-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-72 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B44C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-30 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B44C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-30 |
filingDate |
2013-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86a45be214d7de57f7262414279acb51 |
publicationDate |
2013-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2013109674-A1 |
titleOfInvention |
Method of decorating chemically strengthened glass |
abstract |
A method of decorating chemically strengthened glass. The coating deposition process entails maintaining a deposition temperature and a curing temperature below a threshold where the chemically strengthened glass is weakened. The coating composition used in the process is a single phase and comprises alkoxysilane functionalized isocyanurate or alkoxysilane functionalized biuret, wherein the alkoxysilane is linked to the isocyanurate or biuret by an urea linking group. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023107355-A1 |
priorityDate |
2012-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |