Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_04a25ddcc405fe1eb2c9f5459a07a67b http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aa167897a816e0e598235c706de2c370 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ffb7338f959400a6a869adcec4b4572e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_137ad4f406af5b0333fbe8694f2ed4a9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4ee2c8645e56beaf60f158116aed789c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2c8abd22b36e9c94090f9889ecf27cb5 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-174 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F15-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N27-302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-194 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C245-04 |
filingDate |
2012-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c6efd87d8bab4310c75cb65815f2d0a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_871eb935a4fc63a9adb5ea6b7951e373 |
publicationDate |
2013-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2013093882-A2 |
titleOfInvention |
Derivatization of carbon |
abstract |
Chemical modification of the surface of elemental carbon comprises a first stage of attaching a compound with an azo group to the elemental carbon and then a second stage of decomposing the azo group in the presence of one or more compounds with an olefinic group so that decomposition of the azo group forms radicals attached to the carbon surface and a said radical forms a covalent bond to a said olefinic group. The second stage may proceed as a polymerization of a vinyl monomer with a redox active group such as ferrocene, anthracene or anthraquinone. The resulting polymer-modified carbon may be used in an electrochemical sensor. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015184815-A1 |
priorityDate |
2011-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |