Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b817281c05ac900a51077be51df4ef14 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F05D2230-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F05D2300-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-0005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F05D2300-605 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2081-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-0001 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F04D29-426 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F04D29-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F04D29-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F04D29-2222 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F04D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 |
filingDate |
2012-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ccdd195ebf897f9cb0c9deca7e17a236 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8e3002b211a511ba23a5ca29b472e7e2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4b0d386898682ee17c3696e9906d0ca |
publicationDate |
2013-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2013090168-A1 |
titleOfInvention |
Injection molding of polyarylene sulfide compositions |
abstract |
A method for injection molding a thermoplastic composition that contains a polyarylene sulfide and a boron-containing nucleating agent is provided. By selectively controlling certain aspects of the polyarylene sulfide and nucleating agent, as well as the particular manner in which they are combined, the crystallization properties of the resulting thermoplastic composition can be significantly improved. This allows the "cooling time" during a molding cycle to be substantially reduced while still achieving the same degree of crystallization. The cooling time can be represented by the "normalized cooling ratio", which is determined by dividing |
priorityDate |
2011-12-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |