http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013084836-A4
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c0444efde206a2f829562761e58b7e1e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2924-0002 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L23-293 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L23-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L23-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-16 |
filingDate | 2012-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_777e4c7c4b7ea098e8ee41910238bf00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ed03c3a11720c14526d921e6c14799e |
publicationDate | 2013-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2013084836-A4 |
titleOfInvention | Sheet-shaped coupling agent, coupling method, and manufacturing method for electronic device |
abstract | Provided is a sheet-shaped coupling agent that enables the effective coupling (or sealing) of members to be treated in electronic devices or the like at comparatively low temperatures. The sheet-shaped coupling agent is obtained by forming a polymer into a sheet, and is used for the coupling (or sealing) of electronic components or the like. Said polymer comprises loosely cross-linked soft polymers, has a high molecular weight between crosslinking points, has a prescribed storage modulus at low temperatures and high temperatures, and has a stress relaxation rate of 0.5-30%. The polymer has a storage modulus of 100-5000 MPa at a temperature of 25°C, a storage modulus of 0.01-10 MPA at a temperature of 80°C, and a molecular weight of 8000-30000 between crosslinking points. |