Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e90d00ef430527d53b94701cab1bf36c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c0444efde206a2f829562761e58b7e1e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2045-14327 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2705-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2045-14868 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C37-0082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C45-14311 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-22 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K26-382 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K26-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 |
filingDate |
2012-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c37674f62a44f9c3dd0366eb043028c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b09749c3009b57593974fee857b588f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5fb185e76085afad0cf9de94f0bd3fad |
publicationDate |
2013-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2013077277-A1 |
titleOfInvention |
Composite molding manufacturing method |
abstract |
Provided is a manufacturing method with which composite moldings of increased joint strength between the metal molding and the resin molding are obtained. A composite molding manufacturing method comprising a laser irradiation process of forming multiple independent holes in a dot pattern on the junction surface of the metal molding, and a process of disposing the portion, which comprises the metal molding junction surface in which the multiple independent holes have been formed in a dot pattern, in a metal mold and insert-molding the resin that is to become the resin molding. The composite molding manufacturing method controls the ratio (dep/D) of the diameter (D) of the hole opening to the depth (dep) of the hole when a single hole is being formed in the laser irradiation process so as to be in the range of 1.0 - 10. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015203473-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102021132222-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10588225-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015159642-A1 |
priorityDate |
2011-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |