abstract |
The present invention relates to a film for an inner liner of a tire, comprising: a base film layer having an absolute weight-average molecular weight of 50,000 to 1,000,000; and an adhesive layer. The present invention also relates to a method for manufacturing the film for the inner liner of the tire. The above-described inner liner of the tire can provide superior air-tightness despite having a thin thickness, thereby enabling a lightweight tire, improving the fuel efficiency of a vehicle, enabling easy molding in a tire manufacturing process, and exhibiting superior moldability and mechanical properties such as high durability, fatigue resistance, and superior adhesive force to a tire carcass layer. |