Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_77e231c0aa6ac914fa9b095242e5243e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3da0a01a64947fab8173bbf48b25d226 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T29-49115 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-058 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0423 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0585 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1397 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0565 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0585 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1397 |
filingDate |
2011-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29144d76dc0515b4afa16333cd989eb7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_efe122a28d57bea70ce263f289fe66e6 |
publicationDate |
2012-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2012086258-A1 |
titleOfInvention |
Solid secondary cell using silicon compound and method for producing same |
abstract |
The purpose of the invention is to provide, by using a configuration for a solid secondary cell with low production costs that is also unlikely to cause environmental problems, a silicon compound in the positive electrode and the negative electrode; also provided is a method for producing the same. Provided is a solid secondary cell capable of accomplishing the above by using silicon carbide having the chemical formula Si 2 C as the negative electrode (5), silicon nitride having the chemical formula Si 2 N 3 as the positive electrode (3), and a cationic or anionic nonaqueous electrolyte (4) disposed between the positive electrode (3) and the negative electrode (5). |
priorityDate |
2010-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |