Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cca4984a35761ff9698720511bda30d2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e5e4cc5ed2c77d57b10f0a79db5738e3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_365d7070f1202fd6c57bc7fb6fe87529 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2250-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-7242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-558 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-714 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24992 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-412 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2250-242 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2250-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31924 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0823 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-325 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 |
filingDate |
2011-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_09052254980862e291e2e6d07b88812d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4cd4129e985bd4e945e08f778f4d64c6 |
publicationDate |
2011-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2011129869-A1 |
titleOfInvention |
Melt blends of amorphous cycloolefin polymers and partially crystalline cycloolefin elastomers with improved toughness |
abstract |
A melt-blend resin composition prepared by melt-blending includes from 60 parts to 99 parts per hundred weight resin in the blend of an amorphous cycloolefin polymer composition exhibiting a glass transition temperature in the range of from 30°C to 200°C; and from 40 parts to 1 part per hundred weight resin in the blend of a partially crystalline, cycloolefin elastomer of norbornene and ethylene preferably having a glass transition temperature in the range of from -10°C to 15°C and a crystalline melting temperature in the range of from 60°C to 125°C and a % crystallinity by weight in the range of from 5% to 40%. The partially crystalline, cycloolefin elastomer optionally has a second glass transition temperature at less than -90°C. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019040574-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2741726-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3214125-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-202017006503-U1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015173262-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022076581-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-202016007973-U1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-202016001500-U1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11266567-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016129480-A1 |
priorityDate |
2010-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |