Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7c6bbb32367f44833c53d651c6c5c5e4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e44228d6b03d3d48032bc61f87f49681 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_abe442f25ad4dec24dbb12c837e737a6 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2996 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-76 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C11-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B19-107 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B19-00 |
filingDate |
2010-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f4d7cffe315d8c4572a9b1d2970b5fb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17510b046594c3323f96115ee27b9f78 |
publicationDate |
2011-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2011097777-A1 |
titleOfInvention |
Preparation method of hydrophobic hollow glass micro bead and hydrophobic hollow glass micro bead thereof |
abstract |
A preparation method of low cost hydrophobic hollow glass micro bead by means of spray drying is provided. Said method comprises adding the atomized mixed solution of boric acid, potassium hydroxide, lithium hydroxide and calcium hydroxide into the high-speed stirred water glass solution, then spray drying the solution and modifying the organic silicon surface. The hollow glass micro bead has high yield, low cost and high stability. |