http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011047032-A2

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0bcebe4513c62e459e6e418e1cd45d99
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-32
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-51
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L95-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L19-003
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D195-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L95-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E01C3-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-51
filingDate 2010-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0fdcc29acd39cabeff6c2a8d3defc120
publicationDate 2011-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber WO-2011047032-A2
titleOfInvention Crumb rubber modified asphalt with improved stability
abstract The present invention relates to a method for producing a crumb rubber modified asphalt comprising the steps of: a) heating a pre-selected quantity of asphalt to a temperature of between about 325°F to 55O°F; b) adding crumb rubber and a mineral acid to the heated asphalt with stirring; and c) blowing air through the asphalt, crumb rubber and mineral acid mixture.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110272632-A
priorityDate 2009-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID246854527

Total number of triples: 20.