abstract |
Provided are an asphalt mixture that includes an aggregate, a polyamide resin, and asphalt, wherein the softening point of the aforementioned polyamide resin is 60-150℃ and the proportion of the aforementioned polyamide resin is 3-90 wt.% on the basis of the total amount of the polyamide resin and the asphalt, and a method of paving that uses the asphalt mixture. The asphalt mixture prevents wear from rutting and breakdown due to torsion, and achieves pavement with a strong resistance against oil, so that even if there are oil leaks on the pavement surface, the pavement is protected from breakdown and shielded from the onset of wear due to rutting and torsion. |