Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_063a1b324005ddc15e16e7529c6258c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b7a91d691495eda35081be85d5599fc7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ee795a8d5c3b9b704bb849f3b2b35f48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_af8342b2be3e0cab97cfb82764478614 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f8fd98f65e7804628dd013007da1334f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c194d22a0739d021a5609af9f22dafbc http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_da481ab1e61f1ff8e909b8575d46499f |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J11-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J11-40 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J17-49 |
filingDate |
2010-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c2a3728a6488553b626c815cd0fc27bb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f69bfee02bf50a8e91fb6ba4e0f5e6d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_529c3a3ff1340f7a33730ba9a2bcc40b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b77ead40819cabc669e1479582bbe1e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_baf87a432ae36c4c5e2da51f2e26bdae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_429b56ed4792bb25cafe1176ac7e10e9 |
publicationDate |
2010-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2010095344-A1 |
titleOfInvention |
Plasma display panel |
abstract |
A plasma display panel is provided which includes an improved surface layer and thereby has improved secondary-electron emission characteristics and charge retention characteristics. This plasma display panel therefore can stably exhibit satisfactory image display performances and can stably operate with a low electric-power consumption. Also provided is a plasma display panel which renders a reduction in aging time possible, besides producing those effects. A crystalline film is deposited as a surface layer (protective film) (8) having a thickness of about 1 µm on the side of a dielectric layer (7) which faces a discharge space, the crystalline film comprising CeO2 containing strontium added thereto in a concentration of 11.8-49.4 mol%. This surface layer (8) thereby has improved secondary-electron emission characteristics and improved aging characteristics. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011138870-A1 |
priorityDate |
2009-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |