abstract |
The invention provides a method of increasing the mesopore volume of a porous activated carbon, comprising coating a porous activated carbon with a metal oxide or metal oxide precursor to form a treated activated carbon; and calcining the treated activated carbon, in a dry atmosphere, for a time and at a temperature sufficient to increase the mesopore volume of the treated activated carbon. The invention also provides an activated carbon having a total mesopore volume of at least about 0.10 cc/g and less than about 0.25 cc/g, and a percentage of mesopore volume per total pore volume of at least about 15% and less than about 35%. Activated carbon modified according to the invention, cigarette filters incorporating such activated carbon, and smoking articles made with such filters are included in the invention. |