Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2c3ef203911b7e1c6988aa34361b78a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_66fe4ffb5288f417cd971ab0c5a7b5d8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_14df928cce1112b89356928855b60351 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2011-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2035-0827 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C35-0888 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00442 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-123 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29D11-00298 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B3-0031 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-006 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L11-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B3-00 |
filingDate |
2009-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e0cd426d5cc72e88c76733fb8024cba7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df520f74952d207c0a01188c560e80bf |
publicationDate |
2010-05-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2010050290-A1 |
titleOfInvention |
Wafer lens manufacturing method and wafer lens |
abstract |
Provided is a wafer lens manufacturing method for manufacturing a wafer lens (1) provided with convex lens portions (5) on a glass substrate (3) by curing resin (5A) between the glass substrate (3) and a resin mold (20) in which concave cavities (24) are formed, in which after a tip side molding step is performed one or more times whereby the uncured resin (5A) is disposed on at least the cavities (24) in the resin mold (20) and cured, a base end side molding step is performed whereby the uncured resin (5A) is disposed between the resin mold (20) and the glass substrate (3) and the disposed resin (5A) is cured while being pressed from above by the glass substrate (3). Thus, the wafer lens with desired optical performance and a large amount of sag can be formed while a reduction in productivity is prevented. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10126530-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3431275-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2939053-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9478681-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10386616-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11130299-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017034402-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/NL-2012262-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/NL-2015330-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011177955-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108367515-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108367515-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9649788-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017022190-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015122769-A1 |
priorityDate |
2008-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |