Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f10b24e9c5551fcaef6a5bd99c20d367 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_35c163b846f1e43382aeed8dd7bad2a8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e2e07c69f4b06e5e67e4daf1dbee1c85 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2325-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2203-14 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0019 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F12-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F12-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-14 |
filingDate |
2009-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7382ed8c8f6ddc7ed3d800b31fec4eaa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d07267a7653a2db58fc5b35e3b370065 |
publicationDate |
2009-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2009118251-A1 |
titleOfInvention |
Process for the preparation of expandable polystyrene |
abstract |
The present invention relates to a process for the preparation of expandable polystyrene comprising the following steps : i°) heating an aqueous suspension comprising styrene monomer and at least one organic peroxide initiator of formula (I) 1-alkoxy-1-t-alkylperoxycyclohexane in which the alkoxy group contains 1 to 4 carbon atoms, the t-alkyl group contains 4 to 12 carbon atoms, and the cyclohexane ring may optionally be substituted with 1 to 3 alkyl groups each, independently having 1 to 3 carbon atoms, at a temperature ranging from 100°C to 120°C, ii°) adding a blowing agent selected from the group consisting of alkanes having from 4 to 6 carbon atoms and mixtures thereof. The invention also relates to an expandable polystyrene obtainable according to such a process and to insulation parts and packaging comprising such an expandable polystyrene. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012238685-A |
priorityDate |
2008-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |