Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1fa893ad762099de57d3c9c93b13d968 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_189b6baabadf493babdc2c5681f659b6 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-139 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F236-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C1-15 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C1-15 |
filingDate |
2009-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c2c148f2bf8fbb77b5aae8ef4cfcf4e7 |
publicationDate |
2009-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2009095313-A1 |
titleOfInvention |
Nitrile rubbers which optionally contain alkylthio terminal groups and which are optionally hydrogenated |
abstract |
An improved polymerization and processing method allows the production of special nitrile rubbers which are characterized by a specific cation content which leads to an excellent storage stability and particularly good vulcanization rate and moreover results in vulcanized materials that have advantageous properties. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015101599-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2889326-B1 |
priorityDate |
2008-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |