Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5b059df40fe729bbab6f723bcae9b15f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a13def4caf1c8a1f082ad3613b1a9cd0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-548 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L15-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-548 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-42 |
filingDate |
2008-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b4665d95fefb65c149234b3413904e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e451eac087e305676a82ca8cf40e61a9 |
publicationDate |
2009-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2009084667-A1 |
titleOfInvention |
Tire |
abstract |
Provided is a tire that not only has excellent wear characteristics but also good control stability typified by wet skid resistance and reduced rolling resistance (low heat buildup). The tire is provided using as the tread a rubber composition wherein (B) 20-150 parts by weight of silica wherein the cetyltrimethylammonium bromide (CTAB) adsorption specific surface area is 60-130 (m2/g) and the nitrogen adsorption specific surface area (N2SA) by the BET method is 70-140 m2/g are blended with respect to (A) 100 parts by weight of a rubber component comprising 15-70 wt% of an amine functional group-modified styrene-butadiene copolymer. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010275386-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2012016056-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011122136-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018035240-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2366557-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014002706-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012246333-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013112731-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9663639-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011057980-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2457948-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2457948-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018035241-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102199316-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102199316-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017008161-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013224407-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013133373-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8754159-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012115211-A1 |
priorityDate |
2007-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |