Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e3b3f4f8df8306f743faf2d4a4af65e1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9926f4f81c477e14d77f89f515ffd35c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_05a052a47fcb872e2206023cc294e13f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F232-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-69 |
filingDate |
2008-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1b205fd6c14d7372862fa20b3035909 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b1381db3a124a8bcab0cbb11b61daf84 |
publicationDate |
2009-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2009080438-A1 |
titleOfInvention |
Process for obtaining polymers of ethylene and cycloolefins |
abstract |
A terpolymer containing: a) from 90% to 50% by weight; preferably from 90% to 70 % by weight of ethylene derived units; b) from 5% to 40% by weight; preferably from 5% to 20% by weight of derived units of alpha olefin of formula CH2=CHA wherein A is a C1-C20 alkyl radical; c) from 2% to 30% by weight, preferably from 5% to 20% by weight of cycloolefins derived units. Said terpolymer being characterized by the following features: i) distribution of molecular weight Mw/Mn lower than 3.5; preferably lower than 3; more preferably lower than 2.7; ii) solubility in xylene at 25°C higher than 99%. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011061151-A1 |
priorityDate |
2007-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |