Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d29eb5cbe2c2b3688bb719738b4cc783 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6d6ad677aaba193a6d4dc380380b941d http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95c89084d61fd47ae93470ca7c96f184 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_241e756dd6720a0d0a05d8db263efe9d http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_960ebef85e421e2806bc833a763f8ba4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_943f1bac040f018a45e21b4e3ffe1cb4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-51 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-50 |
filingDate |
2008-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eba509ff0610d7691a5175874fa5f4ae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc521ece9c7acca1cf6708311869102c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_594f9a04690ff51d5ea2f59bd5c86ae2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3298c9c66bee3edbd0a7a62b132d13b9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a292beb0775742f5586819117e37c02 |
publicationDate |
2009-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2009043676-A3 |
titleOfInvention |
Black, method for the production thereof, and use thereof |
abstract |
The invention relates to black having a CTAB surface area of 100 to 160 m²/g, a quartile ratio of more than 1.60, and an FP index of >0. Said black is produced in a furnace reactor. Sixty to 90 percent by weight of the raw black material are injected into the reactor in the first third of the reaction zone, while the remaining amount of the raw black material is injected into the reactor upstream at least in one other point. In addition, the combustible is conducted such that 90 to 100 percent by weight of the combustible are evaporated when first hitting the raw black material and 80 to 99 percent by weight of the combustible are evaporated 5ms before hitting the raw black material. Said blacks can be used in rubber mixtures. |