Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1dbdbd42540fa9bcc9b547f9918dd672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ff33bcec6d3dc188a9a6cb031b9c6dac http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a797f6a460da10ff3f7b20ea90a99869 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B6-443 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B6-4402 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0853 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B6-4429 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0869 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B6-44 |
filingDate |
2007-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0de57f1f317694f9c7864ee41d926d38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e066bbdd4517dd611334355b4e1108a |
publicationDate |
2009-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2009016424-A1 |
titleOfInvention |
Telecommunication cable equipped with tight-buffered optical fibers |
abstract |
The present invention relates to a telecommunication cable equipped with at least one optical fiber coated by a tight buffer layer made from a polymeric material having an ultimate elongation equal to or lower than 100% and an ultimate tensile strength equal to or lower than 10 MPa. The above combination of features of the polymeric material forming the buffer layer allows to obtain an optical fiber which is effectively protected during the installation operations and during use, and at the same time can be easily stripped by the installer without using any stripping tools, simply by applying a small pressure with his fingertips and a moderate tearing force along the fiber axis. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015153323-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10162144-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8265437-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102141664-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011026889-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9857548-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9429730-B2 |
priorityDate |
2007-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |