http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008148870-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_43d5505552431965c7ea915f32646405 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b897e0f5263d943b2219acc661f2fb22 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-061 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-007 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-00 |
filingDate | 2008-06-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b8afdd149b87e0d9f6e7ee1f49ffc41 |
publicationDate | 2008-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2008148870-A2 |
titleOfInvention | Method for producing a coating |
abstract | The invention relates to a method for producing a coating on a base. The method according to the invention comprises the following steps: applying a first synthetic resin; applying a temporary coating component to at least sections of the surface of the first synthetic resin prior to the curing of the first synthetic resin, the temporary coating component not being reactive, being immiscible with the first synthetic resin and having a lower specific weight at least at the time of application than the first synthetic resin; at least partially removing the temporary coating component after the time at which the first synthetic resin is at least cured to such an extent that it maintains its surface structure. |