Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_02823aaee230e671bb5f4eb4a1f8bbe6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_122a60290d36b8fec1f83ffb6b8c1c06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5c47b4cdc70fc324bb60b05d4f833de5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_db1557303947c0c02062da3f6dfe2e6f |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F236-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-005 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-10 |
filingDate |
2007-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e38ffccf141aa127aaca0cac06a2e894 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_149af8b06896df7769303c155db938e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8feda603b80819cd00d7a6e10caf5890 |
publicationDate |
2008-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2008019461-A1 |
titleOfInvention |
Process for obtaining butadiene-styrene copolymers by emulsion polymerization; rheology modifying agent for copolymer; rubber composition; gum base; chewing gum; and bubble gum |
abstract |
The present invention refers to a process for obtaining butadiene-styrene copolymers (SBR) that are prepared by aqueous emulsion polymerization technology, at high temperature, having differentiated rheological properties and which are particularly directed to the industry of manufacturing chewing gum and bubble gum. The present invention also refers to a rheology modifying agent for said butadiene-styrene copolymers, which are derived from the emulsion polymerization process. The present invention also refers to the SBR rubber product, mixture or composition having differentiated rheological properties that is obtained after the step of coagulating butadiene-styrene copolymer (SBR) latex. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2659058-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8637600-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8623972-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2604651-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014086810-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9447263-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104812592-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008122872-A1 |
priorityDate |
2006-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |