Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_39a0d51c2625cda65bce644f99add2ca http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c408adc494397eb1be0ce4c68f1d6e31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4315e79f5edcdb5d96f9e5d64390a852 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1c544b58fee987a3aaf3332b0060366c |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2331-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-061 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4854 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-282 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-70 |
filingDate |
2007-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_327a75aeebb532a2f78ca808bb462268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb024024c5ea770fd694e22a5f2f57b0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbe0c70d594ff495e554510c664b8fa8 |
publicationDate |
2008-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2008007879-A1 |
titleOfInvention |
Polyurethaneurea elastic fiber and method for preparation thereof |
abstract |
The present invention relates to a preparation method of a polyurethaneurea elastic fiber, in which the sub-reaction and reaction speed are regulated during the prepolymer reaction by adding 1- functional monoalcohol and an organic acid in order to provide an elastic fiber exhibiting excellent uniformity during the weaving and processing of a synthetic fiber such as polyester or nylon, a static mixer having excellent stirring efficiency and a tubular reactor are used for constant even reaction to give a primary uniform polymer, the primary polymer is dissolved in a solvent using a high shear mixer, and a chain extender and chain terminator are added with regulation to give the secondary polymer having intrinsic viscosity of at least 1.0. In the present invention, a high shear mixer for the secondary polymerization exhibiting at least 80% of stirring efficiency and a cylindrical pipe shaped static mixer were used to inhibit sub-reaction and gelation to give a secondary polymer exhibiting stable spinning. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8623950-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108505141-A |
priorityDate |
2006-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |