http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008004969-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d90639d4de7b58b780d7f8c01781da4
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f7e4c8dd3a8662733a37ad28493d1333
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2aca6f8e0b792a0742e1fdbff046253f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cdb203edd3aa75a2cf33fb97cf9c510d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_954c0b2d740e873ce81f8b3e03a3ca52
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22D11-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22D11-115
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22D27-02
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D11-115
filingDate 2007-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff6164b4d04a6151a050837bdedbd067
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_939eda603ce637b3ed8eb6130b5516af
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7efade94aa12eb0c02401fdf80ca9be8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f259caf0ee92555ab3199753099abf5a
publicationDate 2008-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber WO-2008004969-A1
titleOfInvention Method and apparatus for controlling the flow of molten steel in a mould
abstract A method for controlling a flow of molten steel in a mould by applying at least one magnetic field to the molten steel in a continuous slab casting machine. This is achieved by comprising controlling a molten steel flow velocity on a molten steel bath surface, meniscus, to a predetermined molten steel flow velocity by applying a static magnetic field to impart a stabilizing and braking force to a discharge flow from an immersion nozzle when the molten steel flow velocity on the meniscus is higher than a mould powder entrainment critical flow velocity and by controlling the molten steel flow velocity on the meniscus to a range of from an inclusion adherence critical flow velocity or more to a mould powder entrainment critical flow velocity or less by applying a shifting magnetic field to increase the molten steel flow when the molten steel flow velocity on the meniscus is lower than the inclusion-adherence critical flow velocity.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2574556-C1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10207318-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8985189-B2
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016078718-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013091701-A1
priorityDate 2006-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000351048-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1486274-A1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID87540
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128727325
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3676
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID87540

Total number of triples: 31.