Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_86f6ef68fc51089e87eb9bdde24e0dd8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_96c412a5b5e753d384703ab9116ccc1a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 |
filingDate |
2007-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1fa5e85a94c20f26c4066e6eae5c6d3d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_082ec3a19567c760212f1937a1cb71f8 |
publicationDate |
2008-01-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2008001612-A1 |
titleOfInvention |
Antireflection film and method for producing the same |
abstract |
Disclosed is an antireflection film comprising a transparent supporting body and an organic-inorganic composite layer directly bonded to the surface of the transparent supporting body. In this antireflection film, the surface of the organic-inorganic composite layer is subjected to a water- and oil-repellent treatment. The refractive index of the transparent supporting body is not less than 1.57. The organic-inorganic composite layer contains an organic portion composed of the polymer of a graft polymer chain and an inorganic portion composed of a crosslinked structure formed by hydrolysis and condensation polymerization of an alkoxysilane. The refractive index of the organic-inorganic composite layer is within the range of 1.35-1.49. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016505162-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012237941-A |
priorityDate |
2006-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |