Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_07d337c967c20c1f1d2d88541b22682e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_509d6313cb788ea6e94fa5f021320c6b http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fc352820376eaa22ac5d978acc02cc1 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-3065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2400-303 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2317-16 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J5-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27M1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27D1-04 |
filingDate |
2006-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b9a1d5e2d76f180db98db272f572de7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f37323a181ece78f1fca395ddfcaeb3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_821dce254ca065a340cbbef5e60f696b |
publicationDate |
2007-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2007147299-A1 |
titleOfInvention |
A method for making fire retardant reconstituted decorative lumber |
abstract |
A method for making fire retardant reconstituted decorative lumber mainly consists in an additional process of the fire retardant treatment on the veneer as compared with the prior method thereof. The fire retardant soaks into the veneer after the fire retardant treatment, resulting in esterification, etherification and graft copolymerization of the groups such as hydroxy group in the lumber, so as to isolate from air, fire seat and flammable gas or to dilute the flammable gas, thus the fire retardant property is obtained, thereby changing the thermal cracking process of the lumber and keeping the lumber combustion in control. Other physicalor chemical properties of the lumber have small changes before and after the treatment. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112873458-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9132569-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112873458-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102490220-A |
priorityDate |
2006-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |