Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4dce8dd4dc10051564aeaa9dc08df67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9e3fec87f16942097a9736f54881be51 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2371-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-2256 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-122 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C41-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-20 |
filingDate |
2007-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2047780a23106a8c38d38023ef8258b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65789bc6ab72cb84b1b57af955f0d1ec |
publicationDate |
2007-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2007114489-A1 |
titleOfInvention |
Solid electrolyte membrane, method and apparatus for producing the same, membrane electrode assembly and fuel cell |
abstract |
In a casting membrane forming process (63), a dope containing a solid electrolyte is cast on a casting belt (93) from a casting die. On the casting belt, a casting membrane (61) is formed. In a casting membrane drying process (66a), the casting membrane (61) is dried. In a solvent contacting process (66b), the casting membrane (61) contacts a poor solvent of the solid electrolyte. By a self-supporting property developing process (66), a self-supporting property is given to the casting membrane (61) for a short time. The casting membrane (61) is peeled from the casting belt (93) as a precursor membrane (67). The precursor membrane (67) is immersed into water. After the precursor membrane (67) is dried, a proton substitution is performed to obtain a hydrogen-substituted membrane (75). By washing and drying of the hydrogen-substituted membrane (75), a solid electrolyte membrane (79) is obtained. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-116111155-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11672684-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11612416-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10349982-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10238427-B2 |
priorityDate |
2006-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |