http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007112349-A2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fbfd4a011eb8265b54e6800d8f9750a8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1543b2b19ec0e331a0dcd89888cbef5f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B19-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C1-008 |
filingDate | 2007-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8eea083d095ba5480552947b15a72b9f |
publicationDate | 2007-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-2007112349-A2 |
titleOfInvention | Production of self-supporting glass film |
abstract | A process is described for production of a self-supporting glass film that includes the steps of preparing a boron-containing aqueous solution containing boric acid and an alkanolamine; producing a mixture that includes the boron-containing aqueous solution, a colloidal silica sol and an organic binder; applying the mixture onto a base material to form a coating; drying the coating to form a precursor film on the base material; releasing the precursor film from the base material; and firing the released precursor film. A self-supporting glass film prepared using this process is also described. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016037707-A1 |
priorityDate | 2006-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 42.