Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5abd6118cc2d561aaf0ab0ab826518e2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_eeee7a954ef2dd0b4fa1a464ac7b7b5c http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e576225e2a3e746eb60e2212aa3fb041 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-85 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-80 |
filingDate |
2007-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f55f07ca02f68c1d5a7f993d79e0c09e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4850cb986a86e4acc6944ab9720296b |
publicationDate |
2007-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2007090885-A1 |
titleOfInvention |
Polyester solid phase polymerization catalyst for low acetaldehyde generating resins |
abstract |
This invention discloses a process for producing a polyester resin having a low acetaldehyde generation rate comprised of the steps of polycondensing the polyester resin in the presence of tin and antimony; wherein the tin is present within the range of 50 to 110 ppm of the polyester resin and the antimony is present from 105 ppm to 265 ppm of the polyester resin, and solid phase polymerizing the polyester resin for sufficient time so as to increase the intrinsic viscosity of the polyester resin by at least 0.15 dl/g. |
priorityDate |
2006-02-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |