Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_72a580a6c9a77f371f21b5866a14ac68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2b30aaab6b2cd23887e078e5c256e027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6e57ebca9d3bac8d8aff29e0b54e7b62 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2327-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-245 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-044 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B21-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-044 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B21-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-19 |
filingDate |
2006-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1590b7066c15c6798a9d42424ba3d3e5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75bc2ad0bf0ab434d74f4bf39f134022 |
publicationDate |
2007-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
WO-2007080681-A1 |
titleOfInvention |
Process for producing crosslinked fluororubber |
abstract |
[PROBLEMS] To provide a process for producing a polyol-crosslinked fluororubber which can realize low-tack properties and has a highly enhanced rubber hardness. [MEANS FOR SOLVING PROBLEMS] The process is characterized by subjecting a fluororubber composition which comprises a polyol-crosslinkable fluororubber, a crosslinking accelerator comprising a quaternary phosphonium salt or a quaternary ammonium salt, and a polyol-type crosslinking agent and in which the weight ratio of the crosslinking accelerator to the polyol-type crosslinking agent, X (crosslinking accelerator/polyol-type crosslinking agent), is 0.90-3.00 in the case of the quaternary phosphonium salt and is 0.4-0.6 in the case of the quaternary ammonium salt to thermal vulcanization with pressing to mold a vulcanizate, subsequently applying a treating liquid obtained by dissolving the polyol-type crosslinking agent and the crosslinking accelerator in a solvent to the surface of the vulcanizate, and then heating the coated vulcanizate at 200-300°C for 1-20 hours. |